Resina de poliéster insaturada de fibra de vidrio tixotrópico
$17001-19 Others
$1688≥20Others
Tipo de Pago: | T/T |
Hafen: | Shanghai Port |
$17001-19 Others
$1688≥20Others
Tipo de Pago: | T/T |
Hafen: | Shanghai Port |
Modelo: TC-K196
CAS No.: 25608-12-2
Other Names: unsaturated polyester resin for boat
MF: C3H5NO)n
EINECS No.: 208-750-2
Type: Synthetic Resin And Plastics
Brand Name: Fullmark
Model Number: TC-196, TC-196
Appearance: Light yellow transparent liquid
Packaging: metal barrel
Usage: unsaturated polyester resin for boat
Net Weight: 220kg
Certificate: Msds
Storage Period: 90 days .but it's 30 days if add thixotropice accelerator
Storage Condition: Below 25℃ in dark
Keywords: unsaturated polyester resin for boat
Place Of Origin: Jiangsu, China
Purity: 61-67%
Brand: Fullmark
Unidades de venta | : | ton |
Tipo de paquete | : | barril de metal |
Descripción del producto de resina de poliéster de poliéster TC-K196
TC196 Resina de poliéster de propósito general presenta una buena impregnación de fibra de vidrio, buena resistencia a los rayos UV y resistencia mecánica.
Propiedades de resina de poliéster no saturadas líquidas
Item |
Unit |
Measured data |
Testing method |
Appearance |
- |
Light yellow transparent liquid |
GB-T 8237.4.1.1 |
viscosity |
25℃,Pa·s |
0.25-0.45 |
GB/T 7193.1 |
Gel time |
25℃,min |
9-17 |
GB/T 7193.6 |
Acid value |
mgKOH/g |
28-36 |
GB/T 2895 |
Solid content |
% |
61-67 |
GB/T 7193.3 |
Tiempo de gel: 50% de peróxido de ciclohexanona: 4%; Acelerador E1: 4%;
Propiedad del cuerpo de fundición de resina
Item |
Measured data |
Unit |
Testing method |
Barcol hardness |
46 |
— |
GB 3854-83 |
Distortion temperature |
66 |
℃ |
GB 1634-04 |
Elongation at break |
1.8 |
% |
GB 2568-95 |
Notes:1)casting body sample preparation method according to GB 8237-87,curing system:hardener 55%MEKPO:2%,promoter E1; 2)post cure system:60℃×2h+80℃×2h. |
Propiedad física FRP
Item |
Unit |
Measured data |
Testing method |
Bending strength |
MPa |
325 |
GB/T2570-95 |
Bending modulus |
MPa |
1.40×104 |
GB/T2570-95 |
Notes:1)casting body sample preparation method according to GB 8237-87,curing system:hardener 55%MEKPO:2%,promoter E1; 2)post cure system:60℃×3h+110℃×3h. |
L IQUID RESINA Y CONDICIONES DE ALMACENAMIENTO
Paced en barril de metal, 220 kg/barril (aproximadamente 55 galones)
Trate de evitar que la resina líquida sea directamente solar y recursos de calor
F Lammable, debe mantenerse alejado del fuego abierto
S Helf Life es de 3 meses menos de 25 ℃
Almacenar y operar en un lugar seco y bien ventilado
Nuestros servicios
Contáctame para más detalles de nuestros productos
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.